SAE AMS5843H

Original price was: $74.Current price is: $44.

Cobalt-Nickel Alloy Corrosion- and Heat-Resistant Bars 19Cr – 36Co – 25Ni – 7.0Mo – 0.50Cb (Nb) – 2.9Ti – 0.20Al – 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated Work Strengthened and Aged

Published by Publication Date Number of Pages
SAE 2022 7

SAE AMS5843H – Cobalt-Nickel Alloy Corrosion- and Heat-Resistant Bars 19Cr – 36Co – 25Ni – 7.0Mo – 0.50Cb (Nb) – 2.9Ti – 0.20Al – 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated Work Strengthened and Aged

This specification covers a high strength corrosion- and heat-resistant cobalt-nickel-chromium alloy in the form of bars 1-3/4 inches (44.4 mm) and under in nominal diameter.